Reinforcing Steel
Hot-Dip Galvanized Reinforcing Steel (Rebar) in Concrete Applications
Galvanized reinforcing steel is effectively and economically used in concrete where unprotected reinforcement will not have adequate durability. The susceptibility of concrete structures to the
ASTM A767 - Galvanizing Steel Bars for Concrete Reinforcement - Rebar
ASTM A767 Standard Specification for Zinc-Coating (Galvanized) Steel Bars for Concrete Reinforcement first and foremost specifies the minimum mass (weight) of zinc coating on reinforcing