Increase Steel Service Life Using Hot-Dip Galvanizing

Increase Steel Service Life Using Hot-Dip Galvanizing written by Laura Hanson December 2015 issue of Structure Magazine
Continue Reading »

A New Generation of Galvanizing

A New Generation of Galvanizing Howard Levine Structure Magazine, August 2015
Continue Reading »

Conservation at Its Best: Reuse Galvanized Steel

During a reconstruction or rehabilitation project, there are often building materials that can be reused in a future project. Reclaiming material from an existing structure is a sustainable option that many specifie...
Continue Reading »

AGA Launches New Mobile Inspection App

The American Galvanizers Association (AGA) continues to move forward with the advancement of technology in order to help the galvanizing community more efficiently receive important information, tools, education as...
Continue Reading »

Durability + Design Article: Cold Steel, Hot Zinc

The AGA's Melissa Lindsley and AZZ Galvanizing Services's Joseph  Langemeier co-authored an article on hot-dip galvanzing featured in the December 2013 issue of Durability + Design. Read it here! (Sign in may be req...
Continue Reading »

Specifying Duplex Systems

Specifying Duplex Systems: Aesthetics and protection with hot-dip galvanized steel and coatings by Melissa Lindsley The Construction Specifier August 2013
Continue Reading »

Hydrogen Embrittlement Study of Hot-Dip Galvanized High-Strength Bolts

This article demonstrates the feasibility of using hot-dip galvanizing to produce corrosion protection for ASTM A490 bolts without making them susceptible to hydrogen embirttlement. by Dr. Tom Langill Fastener Tec...
Continue Reading »

Taking a Dip

Taking a Dip: Hot-dip galvanizing experts answer questions about the zinc-rich protective coating system. by Phil Rahrig and Dr. Tom Tangill Modern Steel Construction November 2012
Continue Reading »